Grade guide · updated 25 November 2026
SS 304 vs SS 202 pipe: which grade should you use?
Both are austenitic stainless steels and look the same when polished. The difference is in what they are made of, and that decides how long they stay bright outdoors.
Short answer: use SS 304 outdoors, near the sea, in kitchens and in public spaces. Use SS 202 for indoor railings, furniture and decorative work where cost matters more and the pipe stays dry.
Composition, side by side
Maximum or range, percent by weight, for the standard grade designations:
| Element | SS 304 UNS S30400 | SS 202 UNS S20200 |
|---|---|---|
| Chromium (Cr) | 18–20 | 17–19 |
| Nickel (Ni) | 8–10.5 | 4–6 |
| Manganese (Mn) | 2 max | 7.5–10 |
| Carbon (C) | 0.08 max | 0.15 max |
| Nitrogen (N) | 0.10 max | 0.25 max |
Source: SAE/AISI stainless designations table [1]. Exact limits vary slightly between standards (for example ASTM A276 lists 8.0–11.0% nickel for 304 bar [2]). For any pipe you buy, the coil's mill test certificate is what counts.
Why the difference matters
SS 202 replaces part of the nickel with manganese and nitrogen. That keeps the steel austenitic and lowers its cost, because nickel is the expensive element. The trade-off is less chromium and nickel, so 202 holds up less well where moisture and salt sit on the surface.
SS 304, the classic "18/8" grade, resists a wide range of everyday atmospheres. It can still pit in warm, salty conditions; for severe marine use, engineers move up to SS 316 [2].
Which grade for which job
| Use | Suggested grade |
|---|---|
| Balcony and terrace railings, gates, outdoor handrails | SS 304 |
| Coastal towns, swimming pools, public spaces, kitchens | SS 304 (or 316 for direct sea spray) |
| Indoor staircase railings, furniture frames, decorative work | SS 202 is usually enough |
| Projects where the specification names a grade | Follow the specification |
This is general guidance from KGV, not an engineering guarantee. Ask your architect or fabricator for critical or structural work.
How to check which grade you were sold
- Ask for the mill test certificate. It lists the coil's chemical composition. Compare the nickel and manganese figures with the table above.
- Use a spectrometer (PMI) test for large orders. Many steel traders and labs offer it.
- Don't rely on a magnet. Both grades are austenitic and mostly non-magnetic; cold forming can make either slightly magnetic.
What KGV plans to make
KGV Stainless is setting up a two-line mill in Rourkela, Odisha for TIG-welded, polished pipe in both grades: round 38.1 mm and square 38.1 × 38.1 mm, 1.5 mm wall, 20 ft lengths. Production has not started yet. Tell us what you need and we will contact you when supply begins.
Sources
- SAE steel grades: stainless steel designations table, Wikipedia (types 202 and 304, composition by weight %). Read 25 November 2026.
- SAE 304 stainless steel, Wikipedia: composition per ASTM A276, and corrosion behaviour in chloride environments. Read 25 November 2026.